MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

3M Scotch® 77 White Fire-Retardant Electric Arc Proofing Tape
Categories: Polymer; Adhesive

Material Notes: Scotch® Fire-Retardant Electric Arc Proofing Tape 77 Series are designed to protect most types of electrical cables from fault arc-generated heat and flames of nearby cable failures. These elastomeric tapes are formulated to generate a thick, insulating charred buildup when exposed to high temperatures. The insulating charred buildup protects wrapped cables and cable accessories from the fault arc-generated heat and flames of cable failures within approximately 20 inches until limiting devices can interrupt the faulted circuit. Because Scotch® Fire-Retardant Electric Arc Proofing Tape 77 Series are elastomeric and unsupported, they are very conformable. Installers can provide virtually wrinkle-free coverage of cables and irregularly-shaped cable accessories, easily and rapidly. This exceptional conformability provides better product control while wrapping and yields more uniform coverage. Also the tape’s thin cross section reduces the overall weight compared to other methods while providing arc protection. The white gray color of Scotch Tape 77 White allows for easy identification of burned areas. One half-lap wrap provides adequate protection for most installations. However, additional wraps can be applied, if conditions warrant, without requiring a reduction in conductor loads.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 762 microns30.0 mil
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break  90 %
@Temperature -18.0 °C
90 %
@Temperature -0.400 °F
ASTM D1000
 130 %
@Temperature -12.0 °C
130 %
@Temperature 10.4 °F
ASTM D1000
 150 %
@Temperature 23.0 °C
150 %
@Temperature 73.4 °F
ASTM D1000
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown >= 10000 V>= 10000 V
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
Flammability, UL94 V-0V-0Self-extinguishing
Oxygen Index 26 - 28 %26 - 28 %ASTM D2863
 
Descriptive Properties
AppearanceWhite-Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch® 77 Black Fire-Retardant Electric Arc Proofing Tape
3M Scotch® 231 Performance Masking Tape
3M Scotch® 226 Solvent Resistant Masking Tape
3M Scotch® 222 High-temperature Fine Line Masking Tape
3M Scotch® 22 Heavy Duty Vinyl Electrical Tape

PMM35195 / 169942

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.