MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Silpak R-1348 Firm Tin RTV Silicone System
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: R-1348 is a 40 Shore A, Tin Base (condensation cure), two-component, room temperature cure (RTV) rubber designed for general purpose applications where a low shrink, firm rubber mold or part is required. Its consistent curing characteristics, excellent shelf life, and outstanding physical properties make it a product that can easily meet a wide variety of applications. Use to cast foam, polyester, urethane, epoxy, low melt metal (350°F), thermoplastics (polyvinyl), wax, soap, plaster, and any material where a release free casting is required.

Features:

  • Extra firmness for casting urethane foam parts
  • Excellent physical properties with high tear resistance
  • Good polyester and urethane resin resistance
Applications: Use to molds cast foam, polyester, urethane, epoxy, low melt metal (350°F), thermoplastics (polyvinyl), wax, soap, plaster, and any material where a release free casting is required.
  • Production molds

Information provided by Silpak a division of Polytek Development Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Viscosity 50 cPInitial Activator
 40000 cPInitial Mixed
 45000 cPInitial Base
Storage Temperature 64.0 - 86.0 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
Tensile Strength 500 psi
Elongation at Break 350 %
Tear Strength 170 pli
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 - 10.0 hour
Pot Life 60.0 min
Shelf Life 6.00 Month
 
Descriptive Properties
ColorOff-White Base; Orange Activator
Mix Ratio100 Base:5 Activatorby weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSILPAK018 / 318655

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.