MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Matexcel BIOT-042 PLA Vascular Tissue Engineering Material
Categories: Wood and Natural Products

Material Notes: BIOT-042; PLA Vascular Tissue Engineering Material; biodegradable material; Biopolymer materials; Tissue Engineering material

Morphology: Hollow Tube

Key Words: Synonyms: PLA Vascular Tissue Engineering Material
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 150 µm150 µmOD; 100um ID
 200 µm200 µmOD; 100um ID
 300 µm300 µmOD; 250um ID
 350 µm350 µmOD; 250um ID
Storage Temperature 4.00 °C39.2 °F
 
Descriptive Properties
Product overviewThis product is a scaffold material for vascular tissue engineering prepared from biodegradable polymer materials. It has good cell compatibility and can be made into a three-dimensional structure similar to the human body. It has porosity requirements for cell growth and vascular mechanical properties requirements.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK2012 / 300643

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.