MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Arya Sasol HBM 5020 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HBM5020 is a high density polyethylene with broad molecular weight distribution, specially developed for small blow molded bottles. This grade offer high stiffness, easy flow, very good ESCR and chemical resistance and sufficient impact strength. HBM5020 is recommended for multipurpose blow molding process. HBM5020 has been manufactured under Basell license.

Application: Multipurpose blow molding process, small blow molded bottles, packaging of consumer and dangerous goods

Forms: Pellets

Attribute: Good ESCR, good chemical resistance, high stiffness

Additives: Antioxidant: Yes; Processing Aid: No; Antiblock: No; Slip Agent: No

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.500 g/cc>= 0.0181 lb/in³ISO 60
Density 0.950 g/cc0.0343 lb/in³ISO 1183
Environmental Stress Crack Resistance 150 hour150 hourBasell method
 6.0 hour
@Pressure 3.50 MPa,
Temperature 80.0 °C
6.0 hour
@Pressure 508 psi,
Temperature 176 °F
FNCT, 2% Arkopal N100; ISO 16770
Melt Flow  0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 22 g/10 min
@Load 21.6 kg,
Temperature 190 °C
22 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 45.0 MPa6530 psiH 132/30; ISO 2039-1
Tensile Strength, Yield 25.0 MPa3630 psiISO 527-1, -2
Elongation at Yield 9.0 %9.0 %ISO 527-1, -2
Modulus of Elasticity 1.00 GPa145 ksiISO 527-1, -2
Tensile Impact Strength 110 kJ/m²
@Temperature -30.0 °C
52.3 ft-lb/in²
@Temperature -22.0 °F
Notched, Type 1, Method 1B; ISO 8256/1B
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C268 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C109 °FISO 75
Vicat Softening Point 78.0 °C
@Load 5.10 kg
172 °F
@Load 11.2 lb
Method A; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 200 °C338 - 392 °FExtruder temperature profile
Melt Temperature 190 - 220 °C374 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARYA014 / 250468

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.