MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Foam-iT!® 10 Rigid Polyurethane Foams
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Product Overview: Smooth-On’s FOAM-iT!™ Series are two-component water blown rigid foams that are versatile and easy to use. FOAM-iT!™ products are available in 3lb., 4 lb., 5 lb., 8 lb., 10 lb.,15 lb. or 26 lb. per cubic foot densities. Parts A and B are measured and mixed in equal amounts by volume (Note: FOAM-iT!™ 8 is measured and mixed 2A:1B by weight). The mixture is then poured into a mold or other form (apply release agent if necessary). The mixture will expand many times original volume (depending on which FOAM-iT!™ product you are using) and develop a uniform cell structure. FOAM-iT!™ 3, 4, 5, 10, 15 and 26 have a handling time of about 20 minutes and reach full cure in 2 hours.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.160 g/cc0.160 g/ccASTM D-1475
Viscosity 400 cP400 cPMixed; ASTM D-2393
 
Processing PropertiesMetricEnglishComments
Cure Time 20.0 min0.333 hourHandling/Tack-Free Time
 120 min2.00 hour
Pot Life 1.50 min1.50 minASTM D-2471
 
Descriptive Properties
Approx. Volumetric Expansion6 times
ColorBeige
Kgs./Cubic Meter160[kg/m³]
Lbs./Cubic Foot10[lb/ft³]
Mix Ratio100A:87Bby weight
 1A:1Bby volume
Specific Volume157[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN166 / 296867

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.