MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Weifang Tianrui Chemical LP530 Acrylic Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Introduction: Acrylic PVC Processing aid Sparking Regulators are the copolymer, which is formed by the ACR monomer with latex, and they are also ultra-high molecular weight polymer with multi-layer structure self developed by us

Characteristics and Application: Acrylic PVC Processing aid Sparking Regulators are specially used in low foam density, such as PVC foam pipes, core pipes, boards and profiles .If you add our products into your production line of low foam density products, they can accelerate the plasticization of PVC, greatly increase the strength of the melting body, thus the foams will distribute well and have the dense air bubbles, obtain more well distributed foamed structure, low density and better surface quality.

Information provided by Weifang Tianrui Chemical Co., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.5 %
Apparent Bulk Density 0.0350 - 0.650 g/cc
Particle Mesh Size 20 Mesh>98% Granularity (percent of pass)
Viscosity Measurement 8.0 - 9.0Intrinsic Viscosity(?)
 
Descriptive Properties
AppearanceWhite Freely Flowing Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWEIFTC030 / 320543

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.