MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Primex Plastics Prime ABS Weather-X 100 Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Prime ABS Weather-X 100 is an ABS substrate with an Acrylic co-extruded cap. If requested a thin layer of Acrylic can be extruded on the back side for rigidizing. It offers good weatherability, chemical resistance, and high gloss with good DOI.

Applications: This product is ideal for outdoor applications such as marine, ATV, RV, Tub & Shower Surrounds or anything where the above characteristics are required.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 in/in
 0.0050 - 0.0080 in/inProcessing
Melt Flow 6.5 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 5940 psiASTM D638
Elongation, Ultimate 29 %ASTM D638
Izod Impact, Notched 5.70 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 202 °F
@Thickness 3.17 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 185 °F
@Thickness 3.17 mm
ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 °FDe-mold
 220 - 300 °FPlug Temperature
 300 - 390 °FSurface Temperature
Mold Temperature 110 - 185 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRIM003 / 278474

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.