MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Ambicat" LE4472 Crosslinking Masterbatch
Categories: Polymer

Material Notes: Ambicat LE4472 is an ambient crosslinking black catalyst masterbatch specially designed to be used with Visico base resins LE4421, LE4423 and ME4425 for insulation of low voltage energy cables. The Visico/Ambicat insulation system is designed to crosslink fast at ambient conditions. It can also be crosslinked in sauna or in hot water. The addition of metal soaps and basic (high pH) components, like some fillers, stearates and UV-stabilizers, will deactivate the catalyst and is not suitable together with Ambicat. To prevent deactivation of the catalyst during coloring, Ambicat compatible color masterbatches are needed.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 - 0.700 g/cc0.0217 - 0.0253 lb/in³ASTM D1895
Melt Flow 100 g/10 min
@Load 21.6 kg,
Temperature 190 °C
100 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Storage Temperature 10.0 - 30.0 °C50.0 - 86.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 15.0 Month15.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9600 / 322957

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.