MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hapco Filter-bond™ E - 3505 Thermoset
Categories: Polymer; Thermoset

Material Notes: Filter-bond™ E-3505 is a two-component, flexible urethane. It exhibits excellent bonding characteristics and has a high viscosity(50,000 cps) to minimize wicking into filter media. The most common applications for E-3505 are potting and sealing filter media.

Filter-bond™ was developed specifically for filtration and ultrafiltration applications. This series includes products that do not contain aromatic amines or carcinogenic or mutagenic materials, systems that can be used to pot moist membrane material in place without foaming, and materials that are easily trimmed when used for pre-potting filters. Filter-bond™ includes a line of flexible and rigid materials to meet a wide variety of filtration applications. All Filter-bond™ products are compatible with Hapco’s MiniFIL™ and RapidFIL™ dispensing machines, which are used for potting or encapsulating various filter media. Hapco’s urethanes and epoxies are widely used in filtration and ultrafiltration manufacturing for sealing, bonding, potting or encapsulating:

  • Water Filters
  • Blood Filters
  • Gas Filters
  • Hepa Filters
  • PPE Filters
  • Biotech Filters
  • Clean Room Filters
  • Wine & Beer Filters
  • Medical Device Filters
  • Pharmaceutical Filters
  • Food Processing Filters

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D-4669
Viscosity 43000 - 57000 cP43000 - 57000 cPASTM D-4878
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 85 - 9585 - 95ASTM D-2240
Tensile Strength 10.3 MPa1500 psiASTM D-638
Elongation at Break 200 %200 %ASTM D-638
Modulus of Elasticity 0.0214 GPa3.10 ksiASTM D-638
Izod Impact, Notched NBNBASTM D-256
Izod Impact, Unnotched NBNBASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C122 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Gel Time 45.0 min
@Load 0.100 kg
45.0 min
@Load 0.221 lb
ASTM D-2971
 
Descriptive Properties
Color (cured)Transparent / Hazy
Mix Ratio100:14Weight
 100:17Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHAPCO058 / 317117

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.