MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Vinyl Flexible C80A0  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded; PVC, Flexible Grade

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
 73
@Time 15.0 sec
73
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 10.3 MPa1490 psi510 mm/min; ASTM D638
Tensile Stress at Strain 5.52 MPa
@Strain 100 %
801 psi
@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 350 %350 %510 mm/min; ASTM D638
Tear Strength 41.9 kN/m239 pliDie C, 510 mm/min; ASTM D624
Compression Set 40 %
@Temperature 23.0 °C,
Time 79200 sec
40 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus  0.124 GPa
@Temperature 23.0 °C
18.0 ksi
@Temperature 73.4 °F
ASTM D1043
 0.310 GPa
@Temperature -40.0 °C
45.0 ksi
@Temperature -40.0 °F
ASTM D1043
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -37.8 °C-36.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Melt Temperature 174 - 179 °C345 - 354 °F
 
Descriptive Properties
FeaturesGood Adhesion
FormsPellets
Processing MethodCoextrusion
 Extrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConstruction Applications
 Seals
 Weatherstripping

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AlphaGary PVC AG K580A Q2 Polyvinyl Chloride Thermoplastic
Geon® Performance Solutions Vinyl Flexible R 980A Polyvinyl Chloride, Flexible
Axiall 53080A Moldings & Extrusions Flexible PVC
BorsodChem ONGROVIL S-5070 Suspension PVC-Resin
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade

PH1PN8455 / 102291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.