MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Dyneon™ Dynamar™ FX 5911 Polymer Processing Additive  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Fluoropolymer

Material Notes: Dynamar FX 5911 is a free-flowing fluoropolymer processing aid that is designed for use at very low levels (typically 250-1000 ppm) necessary to improve processing, it does not alter or detract from the good physical properties associated with high strength plastics.

Features and Benefits

  • Broadens extrusion processing capabilities of polyolefin resins
  • Reduces or eliminates die build-up
  • Ideal for use in high viscosity, high molecular weight polyolefins
  • Excellent thermal stability for high temperature processing
  • Lowers apparent melt viscosity
  • For use at very low levels
  • Free-flowing fluoropolymer processing aid
  • Can offer performance and cost advantages

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 - 1.96 g/cc1.90 - 1.96 g/cc
Particle Size <= 2400 µm<= 2400 µm98%
Melt Index of Compound 5.0 - 14 g/10 min
@Load 5.00 kg,
Temperature 265 °C
5.0 - 14 g/10 min
@Load 11.0 lb,
Temperature 509 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 126 °C230 - 259 °F
 
Descriptive Properties
Active Ingredients (%)100
ColorClear to off-white
FormFree flowing granular

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ FX 5920A Polymer Processing Additive
CIMBAR CAL-BEN™ Calcium Bentonite
DuPont™ Kevlar® 49 Aramid Fiber
Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si), Aged
Mueller Ecostream™ GreenDrop™ C27450 Lead Free Plumbing Brass

PDYNE156 / 34964

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.