MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ExxonMobil Bicor® 140 BSR-ONE OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor BSR-ONE is a two-side sealable, one side treated, coextruded OPP film designed for unsupported plain or surface print applications, and in laminations on both HFFS and VFFS packaging machines.

Availability: Latin America, North America and South America

Key Features:

  • Excellent machinablity
  • Stable COF
  • Excellent hot tack
  • Excellent hot slip
  • Excellent hot jaw release
  • Excellent heat seal strength
  • Wide heat seal range on the untreated side (80°F/45°C)
  • Non-migratory slip system for consistent COF
Features:
  • In Lamination Lap Sealable
Applications:
  • Bakery
  • Biscuts/Cookie/Crackers
  • Box Overwrap
  • Confectionery, Gum
  • Confectionery, Sugar
  • Crips and Snacks
  • Frozen Food
  • Pet Food
Uses:
  • Box Overwrap Flexible Packaging
  • HFFS Flexible Packaging
  • Pre-made Bags – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print Unsupported

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 3.70 g/m²/day
@Temperature 38.0 °C
90% RH; 518
Thickness 1.40 milNominal
Coating Weight 19.6 lb/ream520
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.34Treated; 430
 0.39Untreated; 430
Film Tensile Strength at Break, MD 16500 psi20 in/min, 2.0 in Jaw Separation; 510
Film Tensile Strength at Break, TD 37000 psi20 in/min, 2.0 in Jaw Separation; 510
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 5.0 %
@Temperature 135 °C
438
Shrinkage, TD 4.5 %
@Temperature 135 °C
438
 
Optical PropertiesOriginal ValueComments
Haze 2.3 %444
Gloss 85 %45°, Treated Surface; 442
 
Descriptive Properties
Crimp Seal MST216°Funtreated
 234°Ftreated
Crimp Seal Strength650, g/in250°F, 20psi, 3/4sec
Wetting Tension0.8receding COS thetaTreated Surface
Yield22000 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil PP4792E1 Polymer Grade for Oriented Film
ExxonMobil PP4772 Polymer Grade for Oriented Film
ExxonMobil Bicor™ 52MBR666 OPP Film
ExxonMobil Bicor™ 42MB777 OPP Film
ExxonMobil Bicor™ 40MB666 OPP Film

PEXB407 / 37712

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.