MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Eastar GN077 Copolyester, Natural  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Eastar Copolyester GN077 is an amorphous resin with good melt strength, chemical resistance, high clarity and gloss. It is an excellent choice for extrusion blow molding small to intermediate size containers. Film and optical properties measured at a thickness of 10 mils.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccASTM D1505
Water Vapor Transmission 0.490 g/m²/dayASTM F372
Oxygen Transmission 23.0 cc-mm/m²-24hr-atmASTM D3985
Viscosity Measurement 0.70Inherent; EMN-A-AC-G-V-1
Thickness 254 micronsASTM D374
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 22.0 MPaASTM D638
Tensile Strength, Yield 51.0 MPaASTM D638
Elongation at Break 184 %ASTM D638
Flexural Yield Strength 73.0 MPaASTM D790
Izod Impact, Notched 0.400 J/cm
@Temperature -40.0 °C
ASTM D256
 65.0 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Puncture Energy 24.0 J
@Thickness 3.20 mm,
Temperature -40.0 °C
max load; ASTM D3763
 33.0 J
@Thickness 3.20 mm,
Temperature 23.0 °C
max load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 74.0 °C1kg load; ASTM D1525
Glass Transition Temp, Tg 75.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 0.70 %ASTM D1003
Gloss 166 %at 60°; ASTM D2457
Transmission, Visible 67 %Transparency; ASTM D1746
 89 %Regular Transmittance; ASTM D1003
 92 %Total Transmittance; ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Eastar GN078 Copolyester, Natural
Eastman Eastar GN071 Natural PETG Copolyester
Eastman Eastar GN002 Copolyester, Natural
Eastman Eastar GN046 Copolyester, Natural
Covestro Makroblend® UT203 PC+PET

PE9042 / 35098

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.