System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
NuSil CV-2568 Silicone, Two Part Adhesive and Sealant
Categories:
Polymer
;
Adhesive
;
Thermoset
;
Silicone
Material Notes:
General Purpose: Two Part Adhesive and Sealant
Comments: Long Worktime, Low Density
Cure system: Alkoxy
Information provided by NuSil
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
0.664
g/cc
0.664
g/cc
Viscosity
125000
cP
125000
cP
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
50
50
Tensile Strength at Break
1.20
MPa
174
psi
Elongation at Break
60 %
60 %
Shear Strength
0.690
MPa
100
psi
Lap, Primed with SP-120
Electrical Properties
Metric
English
Comments
Dielectric Strength
25.5
kV/mm
648
kV/in
Thermal Properties
Metric
English
Comments
CTE, linear
180
µm/m-°C
100
µin/in-°F
Processing Properties
Metric
English
Comments
Cure Time
10100
min
@Temperature 25.0 °C
168
hour
@Temperature 77.0 °F
Descriptive Properties
Color
Red
Mix Ratio
100:0.5
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
NuSil CV-2566 Silicone, Two Part Adhesive and Sealant
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Master Bond Mastersil 410 One Component Room Temperature Curing Silicon
NuSil CV-2510 Silicone, Two Part Adhesive and Sealant
NuSil CV10-2568 Silicone, Two Part Adhesive and Sealant
PNUSIL175 / 141899
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.