MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Plastics Group Polifil® C-20 20% Calcium Carbonate-Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Calcium Carbonate (CaCO3) Filler

Material Notes: Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resistance to environmental stress-cracking, good surface and low mold shrinkage.

Applications:

  • Appliances
  • Electrical components
  • Housewares
  • Toys
  • Automotive
  • Utility products

Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Density 1.05 g/ccASTM D792
Filler Content 20 %ASTM D2584
 20.0 %TPG WI
Water Absorption 0.000 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.010 cm/cm
@Thickness 1.59 mm
ASTM D955
 0.0130 in/in
@Thickness 3.17 mm
ASTM D955
Melt Flow 8.0 - 12 g/10 min230/2.16; May be specified; ASTM D1238
 8.00 - 12.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 98ASTM D785
Hardness, Shore D 74.0ASTM D1415
Tensile Strength at Break 4000 psiASTM D638
Tensile Strength 4100 psiASTM D638
Elongation at Break 4.00 %ASTM D638
Elongation at Yield 7.00 %ASTM D638
Tensile Modulus 240 ksiASTM D638
Flexural Strength 5500 psiASTM D790
Flexural Modulus 270 ksitangent; ASTM D790
 280000 psiTangent; ASTM D790
Izod Impact, Notched 0.570 ft-lb/inASTM D256
 0.750 ft-lb/inAt 73°F; ASTM D256
Izod Impact, Unnotched 12.0 ft-lb/inAt 73°F; ASTM D256
Gardner Impact 0.725 ft-lbASTM D3029
 40.0 in-lb
@Thickness 12.7 mm
tup; ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °FASTM D648
 210 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °FASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 410 °F
Middle Barrel Temperature 410 - 430 °F
Front Barrel Temperature 430 - 450 °F
Nozzle Temperature 440 - 450 °F
Melt Temperature 400 - 500 °F
Mold Temperature 50.0 - 80.0 °F
Drying Temperature 180 - 220 °C
@Time 3600 - 7200 sec
Back Pressure 50.0 - 100 psi
Screw Speed 50.0 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 141 UV  Polypropylene (PP) Calcium Carbonate 20% - UV Stable
Omni Plastics OmniPro™ HPP CCF20 Homopolymer Polypropylene, 20% Calcium carbonate filled
Global CPP-120 20% CaCO3 Filled, Polypropylene
Avient Maxxam™ PPH-20C Black PP Homopolymer with 20% Calcium Carbonate
Adell RZ-14 Copolymer Polypropylene, 20% Calcium Carbonate Filled

PPOLI011 / 56915

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.