MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Performance Alloys MoldStar® 21 (PAS 21) Bronze Mold Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.

Applications:

  • Lifter Blades
  • Slides
  • Gibs
  • Wear Plates
  • Ejector Sleeves and Bushings
  • Guide Pin and Leader Pin Bushings

Information provided by Performance Alloys.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.260 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 2863000kg
Hardness, Rockwell C 29
Tensile Strength at Break 110000 psi
Tensile Strength, Yield 60.0 ksi
Elongation at Break 1.0 %in 2"
Compressive Strength 61.0 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 300 BTU-in/hr-ft²-°F
@Temperature 15.6 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 12.8 %
Copper, Cu 80.2 %
Iron, Fe 4.5 %
Other 2.5 %
 
Descriptive Properties
Thermal diffusivity at 68°F0.62 ft²/hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Ampco Metal AMPCOLOY® 95 Cobalt-Copper Alloy, Extrusion, >50.8 mm.
Ampco Metal AMPCOLOY® 944 MoldMATE Nickel-Copper
Ampco Metal AMPCOLOY® 91 Beryllium Copper, Extrusion >35mm
Ampco Metal AMPCOLOY® 89 Beryllium Copper, Extrusion

NPER03 / 18770

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.