MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bangtai 76T90M Polyether Based TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Processing: Outstanding resistance to low temperature and hydrolysis, Good weather resistance.

Applications: Electrical wires and cables, Soft oil pipelines, Oil pipelines, Shale gas hoses, Protective cover for signal transmission line, Fire hoses, Water sports equipment etc.

Information provided by Baoding Bangtai Polymeric New-materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.24 g/cc0.0434 - 0.0448 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 88 - 9288 - 92ASTM D2240
Tensile Strength 25.0 - 35.0 MPa3630 - 5080 psiASTM D412
Elongation at Break 450 - 750 %450 - 750 %ASTM D412
100% Modulus 5.00 - 11.0 MPa725 - 1600 psiASTM D412
300% Modulus 12.0 - 18.0 MPa1740 - 2610 psiASTM D412
Tear Strength 78.5 - 137 kN/m448 - 784 pliASTM D624
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 - 210 °C392 - 410 °F
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBANGT044 / 312404

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.