MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

MetalTek MTEK 15-65 Cast UNS N06006 Heat Resistant Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; Cast Stainless Steel

Material Notes: For severe hot gas corrosion resistance at higher temperatures.

Applications: Hearth plates, muffles, roller hearths, carburizing boxes.

Information provided by MetalTek

Cast UNS N06006; Cast Grade HX; Cast ASTM A297

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 415 MPa>= 60200 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1150 °C2100 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.35 - 0.75 %0.35 - 0.75 %
Chromium, Cr 15 - 19 %15 - 19 %
Iron, Fe 7.75 - 20.65 %7.75 - 20.65 %As Balance
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 64 - 68 %64 - 68 %
Silicon, Si <= 2.5 %<= 2.5 %
 
Descriptive Properties
Heat TreatmentNot Heat Treated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlson C 601 Nickel-Chromium-Iron Alloy
Sandvik Sanicro 71 Covered Electrodes
Special Metals INCOLOY® Alloy 800
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel
Bohler-Uddeholm M300 Modified 420

NMETEK099 / 18349

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.