MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES Luriblend® PPS/F GF30 TL15 BK 30% Glass Filled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Additive: PTFE Lubricant

Features: Lubricated, Good Wear Resistance and Low Friction

Appearance: Black

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccASTM D792
Water Absorption 0.030 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 23000 psiASTM D638
Elongation at Break 1.5 %ASTM D638
Flexural Strength 25200 psiASTM D790
Flexural Modulus 2.05e+6 psiASTM D790
Izod Impact, Notched 0.600 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 3.80 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Coefficient of Friction, Dynamic 0.14ASTM D1894
Coefficient of Friction, Static 0.11ASTM D1894
K (wear) Factor 70.0 x 10-10 in³-min/ft-lb-hr
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 8.00 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 500 °FUnannealed; ASTM D648
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1301/GF/30/TF/15 PPS, linear with glass fiber and PTFE
Syensqo (Solvay Specialty Polymers) Primef® 5084 30% GF PPS, Lubricated Grade
LATI Latilub 80-15T G/30 PPS, 30% Glass Fiber Reinforced, PTFE Filled
RTP Company RTP 1305 TFE 10 Polyphenylene Sulfide (PPS); Glass Fiber - PTFE Lubricated
RTP Company RTP 1305 C TFE 15 Polyphenylene Sulfide (PPS); Glass Fiber Reinforced - PTFE Lubricated

PTPC0902 / 136840

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.