MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Synthos CM1000 Chlorinated Polyethylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chlorinated polyethylene is a heat, weathering and oil resistant elastomer that has used in many wire/cable, hose, automotive and industrial parts for many years.

Characteristics: Highest molecular weight, outstanding mechanical performance, excellent low temperature property, improved oil resistance and high filler absorption

Application: Specially designed for magnetic rubber application, especially for oil and heat resistance magnetic rubber application.

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.20 %0.20 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5454
Tensile Strength 12.0 MPa1740 psi
Elongation at Break 850 %850 %
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 1.00 J/g0.430 BTU/lb
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 35 %35 %
 
Descriptive Properties
AppearanceWhite powder
Content10 piece/100gImpurity particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUNDOW236 / 320267

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.