MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LLDPE LL 1201XV Linear Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE)

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
  • Bread Bags
  • Food packaging
  • Form Fill and Seal Packaging
  • Garment Film
  • General Packaging
  • Industrial Packaging
  • Label Film
  • Multilayer Packaging Film
  • Overwrap Film
  • Packaging Films
  • Produce Bags
  • Shoppers
  • Shrink Film
  • Stand Up Pouches
  • Trash Bags
  • Zipper Bag

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccExxonMobil method
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 620 %ASTM D882
Film Elongation at Break, TD 910 %ASTM D882
Elmendorf Tear Strength MD 50 gASTM D1922
Elmendorf Tear Strength TD 450 gASTM D1922
Dart Drop Test 70.0 gASTM D1709A
Film Tensile Strength at Break, MD 8700 psiASTM D882
Film Tensile Strength at Break, TD 6100 psiASTM D882
1% Secant Modulus, MD 44000 psiASTM D882
1% Secant Modulus, TD 48000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 253 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesOriginal ValueComments
Haze 12 %ASTM D1003
Gloss 53 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil HD 6207 High Density Polyethylene Resin
ExxonMobil HD 5404 High Density Polyethylene Resin
ExxonMobil LD 07523.AC Low Density Polyethylene Resin
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade)
Equate EFDC-7087 LLDPE Film Extrusion Resin

PEX99186 / 175422

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.