MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lendell Supersoft Foams
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Angel Skin

This line of foam has excellent feel and touch characteristics, as well as absorbency. The "breath-ability" of these foams, due to their high moisture vapor transmission qualities and the soft feel makes them ideal for skin contact applications. The foam is also formulated for use in the medical field.

Applications:

Outdoor Apparel, Boots, Gloves, Skin Contact Applications, Bed Comforters, Ski Goggles Lense Cleaner, Foam with Metal Dust, "New Grit" Abrasive Foam Blocks, Mattresses and Pillows

Information provided by Lendell Manufacturing Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.30 lb/ft³
Water Absorption 8.5 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 11.8 psiASTM D3574
Elongation at Yield 382.6 %
Tear Strength 3.30 pliDie "C", average; ASTM D3574
 5.00 pliAverage; ASTM D3574
 <= 5.10 pliMax.; ASTM D3574
Compression Set 7.3 %50%; 1H%ct
 16.1 %50%; 1H%cd
 32.4 %50%; 2E%ct
 35.7 %50%; 1A%ct
 81.4 %50%; 1A%cd
 87.3 %50%; 2E%cd
 
Descriptive Properties
CLD 50%0.3
CLD 50% R0.3
Comfort Factor0.2
Expansion, %9in Isopropyl Alcohol
Hysteresis17.1
IFD 25% R5.7ASTM D3574
IFD 25% RRT4.7ASTM D3574
IFD 65%31.9ASTM D3574
Recovery82.9
Sag Factor5.6
Water Retention, %2.6
Wet Out, minutes5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mearthane Durethane™ C Foams DCF and DCM Polyurethane
ExxonMobil LD 503.LN Foams and Compounding Resin
Lendell Medisponge®
Lendell Nolatex® Latex Free Foam
J6 Polymers JFOAM™ FA-210 Engineered Specialty Foam

PLEND03 / 50778

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.