MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NRI Thermo-Fill™ Titanium Reinforcement
Categories: Polymer

Material Notes: Description: Thermo-FillTM is a two-part, titanium-reinforced epoxy putty designed to bond and repair materials that will be exposed to high temperatures. Thermo-Fill contains no solvents, is non-toxic and easily prepares for application in a variety of industrial maintenance applications. Unlike liquid epoxies, Thermo-Fill will not drip or sag. When fully cured, it produces a durable, resilient bond resistant to hydrocarbons, ketones, alcohols, esters, halocarbons, aqueous salt solutions and dilute acids and bases.

Typical Applications:

  • Fills corrosion voids
  • Designed for high temperature applications
Benefits:
  • High temperature resistance
  • No shrinking or pulling away
  • No drips or mess
  • No tools required

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.98 g/cc
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D2240
Compressive Strength 8000 psiASTM D695
Shear Strength 750 psiLap; ASTM D2240
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 300 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 232 °CContinuous
 260 °CIntermittent
Minimum Service Temperature, Air -40.0 °CContinuous
 -40.0 °CIntermittent
 
Processing PropertiesOriginal ValueComments
Working Life 1.50 - 2.00 hour
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy
Overview of materials for Epoxy, Electrically Conductive
Overview of materials for Epoxy, Cast, Unreinforced
Overview of materials for Epoxy Molding Compound
LKAB Minerals MicroCarb Chalk

PNRI022 / 192038

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.