LCM manufactures a wide range of high purity rare earth metals plus yttrium and scandium. The metals are produced by reduction of suitable precursor materials followed by vacuum remelting and/or sublimination to give required purities. Form: Typically supplied in the form of irregular, broken or cropped ingot pieces. |