MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

UBE V215 Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical properties including transparency and glossiness, and making the material ideal for further processing.

Transparency:Superior transparency and glossiness even for applications involving processing of thick objects.

Ease of Processing: Excellent fluidity and melt tension characteristics suited to a wide range of molding methods.

  • Inflation molding - can be molded into even thick or wide products with superior bubble stability.
  • Extrusion lamination - can be drawn down even at high speed.
  • Blow molding - can be molded producing a very smooth surface.
  • Injection molding - can be molded even into very thin products.

Strength: Good balance in length and breadth with superior tearing strength lengthways.

Application: Stretch

Features: High transparency

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D1505
Vinyl Acetate Content 15 %15 %Ube method
Melt Flow 2.0 g/10 min2.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9292ASTM D2240
Tensile Strength at Break 21.0 MPa3050 psiASTM D638
Elongation at Break 740 %740 %ASTM D638
Flexural Strength 60.0 MPa8700 psiOlsen; ASTM D747
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 68.0 °C154 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
UBE B128 Polyethylene
ExxonMobil LDPE LD 637.LI Low Density Polyethylene Resin
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin

PUBE032 / 71592

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.