This product has been designed as a ‘one part system’ alternative to the traditional two part system, C2061103D7 (basecoat) and C2060217D3 (topcoat). It is a screen printing ink for coating barium titanate PTC ceramic substrates. Screen Printing Equipment: semi-automatic, manual Screen Types: stainless steel, polyester, mesh 156-325 tpi Substrate: Barium Titanate PTC ceramic partsInformation provided by Gwent Electronic Materials Ltd. |