MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Redwood Plastics EXTREN® SERIES 500/525 PLATE Fiberglass Structural Shapes, 3/16" - 3/8" (4.76-9.5mm)
Categories: Ceramic; Glass; Glass Fiber

Material Notes: The features of EXTREN® fiberglass structural shapes are readily translated into user benefits:
  • Corrosion Resistant
  • Low in Conductivity — Thermally and Electrically
  • Nonmagnetic — Electromagnetic Transparency
  • Lightweight — Weighs 80% less than Steel
  • High Strength
  • Dimensional Stability
  • Low Maintenance
  • Custom Colors

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.66 - 1.88 g/ccASTM D570
Water Absorption <= 0.60 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 40
Tensile Stress 10000 psiCW; ASTM D638
 20000 psiLW; ASTM D638
Tensile Modulus 900000 psiCW; ASTM D638
 1.80e+6 psiLW; ASTM D638
Flexural Strength 13000 psiCW; ASTM D790
 24000 psiLW; ASTM D790
Flexural Modulus 800000 psiCW; ASTM D790
 1.10e+6 psiLW; ASTM D790
Compressive Strength 16500 psiCW; ASTM D695
 24000 psiLW; ASTM D695
Compressive Modulus 900000 psiCW; ASTM D695
 1.80e+6 psiLW; ASTM D695
Bearing Yield Strength 32000 psiLW; ASTM D953
Poissons Ratio 0.31LW; ASTM D3039
Izod Impact, Notched 5.00 ft-lb/inCW; ASTM D256
 10.0 ft-lb/inLW; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 35.1 V/milLW; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 8.00 µm/m-°CASTM D696
Flammability, UL94 V-0
@Thickness 3.17 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW104 / 296670

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.