MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Chemlon® 109-33 GH Nylon 66, 33% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Notes: High-Impact; Reinforced with 33% Glass Fibers; Highly toughened compound exhibiting strength and rigidity

Features: Good Creep Resistance; Good Stiffness; High Strength; Good Impact Resistance; Good Toughness; Good Processability; Heat Stabilized

Processing Method: Injection Molding

Forms: Pellets

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/ccASTM D792
Water Absorption 0.80 %0.80 %24 hr; ASTM D750
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 138 MPa20000 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 203 MPa29500 psiASTM D790
Flexural Modulus 6.89 GPa1000 ksiASTM D790
Izod Impact, Notched 1.60 J/cm
@Temperature 22.8 °C
3.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 246 °C475 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 293 °C560 °F
Middle Barrel Temperature 282 °C540 °F
Front Barrel Temperature 277 °C530 °F
Nozzle Temperature 277 °C530 °F
Mold Temperature 60.0 - 93.3 °C140 - 200 °F
Drying Temperature 65.6 - 82.2 °C150 - 180 °F
Moisture Content 0.20 %0.20 %
Injection Pressure 34.5 - 138 MPa5000 - 20000 psi
Screw Speed 60 - 120 rpm60 - 120 rpm
 
Descriptive Properties
AppearanceBlack; Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Ascend Performance Materials Vydyne® R533 NAT Nylon 66, 33% Glass Filled
PTS Trimid® N66-G33 33% Glass Fiber Reinforced Nylon 6/6
Americhem Engineered Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled
Plastcom SLOVAMID 6 GF 33 PA6, 33% glass fibre

PTEKNO434 / 128611

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.