MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik ULTRASIL® 7000 GR Silica
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: ULTRASIL® 7000 GR is a precipitated silica for use as a reinforcement filler in the rubber industry.

Properties and applications: ULTRASIL® 7000 GR is a mechanically compacted granulate. On account of the granulation process it leads to less dust development during mixing. ULTRASIL® 7000 GR is easily dispersible and highly reinforcing silica which was especially developed for application in low rolling resistant passenger car tire tread compounds. It imparts to tread compounds high abrasion resistance combined with excellent rolling resistance and wet traction. To achieve these properties it is necessary to use ULTRASIL® 7000 GR and a bifunctional organosilane, such as Si 69®, Si 75®, Si 266® or Si 363. Additionally, the use of diethylene glycol, triethanolamine or other alkaline accelerators might be necessary in order to achieve optimum rubber-technical data.

Application fields are: Tires, mechanical rubber goods

CAS No: 112926-00-8 and 7631-86-9

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.260 g/cc0.00939 lb/in³Poured; ASTM D1513
Particle Size <= 75 µm<= 75 µm<10% SA Ro-Tap; ISO 5794-1F
 >= 300 µm>= 300 µm>80% SA Ro-Tap; ISO 5794-1F
pH 6.56.55% in water; ISO 787-9
Specific Surface Area 160 m²/g160 m²/gCTAB; ISO 5794-1G
 175 m²/g175 m²/gN2; ISO 9277
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Fe (Iron) <= 400 ppm<= 400 ppm
 
Component Elements PropertiesMetricEnglishComments
SiO2 >= 97 %>= 97 %based on ignited substance (2 h/1000°C); ISO 3262-19
 
Descriptive Properties
Content<6 ppmMn
 <6 ppmCu
Electrical conductivity<1300 µS/cm4% in water, ISO 787-14
Loss on drying0.0552 hrs at 105°C, ISO 787-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIN016 / 317050

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.