MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese SO.F.TER Pibiflex® 4612 NAT Copolyester TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Injection Molding Thermoplastic Copolyester Elastomer

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Water Absorption 0.80 %
@Temperature 23.0 °C,
Time 86400 sec
0.80 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4646ASTM D2240
Tensile Strength 25.0 MPa3630 psiASTM D638
Elongation at Break 800 %800 %ASTM D638
Flexural Modulus 0.125 GPa18.1 ksiASTM D790
Izod Impact, Notched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256/A
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ASTM D256/A
Tear Strength 85.0 kN/m485 pliASTM D624
Taber Abrasion, mg/1000 Cycles 85
@Load 1.00 kg
85
@Load 2.20 lb
h18 wheel
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  >= 1.00e+11 ohm-cm
@Temperature 100 °C
>= 1.00e+11 ohm-cm
@Temperature 212 °F
ASTM D257
 >= 1.00e+13 ohm-cm
@Temperature 23.0 °C
>= 1.00e+13 ohm-cm
@Temperature 73.4 °F
ASTM D257
Dielectric Constant  4.21
@Frequency 100000 Hz
4.21
@Frequency 100000 Hz
ASTM D150
 4.25
@Frequency 1000 Hz
4.25
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
@Thickness 2.00 mm,
Temperature 23.0 °C
432 kV/in
@Thickness 0.0787 in,
Temperature 73.4 °F
ASTM D149
Dissipation Factor  0.0060
@Frequency 1000 Hz
0.0060
@Frequency 1000 Hz
ASTM D150
 0.016
@Frequency 100000 Hz
0.016
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 194 °C381 °FASTM D3417
Deflection Temperature at 0.46 MPa (66 psi) 54.0 °C129 °FASTM D648
Vicat Softening Point 148 °C298 °F120°C/h at 10 N; ASTM D648
Oxygen Index 20 %20 %ASTM D2863
 
Descriptive Properties
Fatigue Resistance (mm/1000 cycles).1/300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Flexalloy® 9607-96 Flexible Polyvinyl Chloride
Polymer Industries Polyslick UHMW Rod
Polymer Industries Polyslick UHMW Profile
Overview of materials for Polyether Ester Elastomer
Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE)

PSOFS779 / 162243

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.