MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Adstif HA 612M Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Adstif is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability.

Adstif HA612M is a high crystallinity medium fluidity polypropylene homopolymer. It does not contain slip or anti-blocking additives and it does not contain Calcium Stearate. Adstif HA612M is typically used for cast film applications where high rigidity and high temperature resistance are required. Adstif HA612M is used for the production of coextruded twist wrapping, labels, lamination, metallize able film and textile packaging. Films produced with Adstif HA612M have been reported by customers to exhibits very high stiffness. Applications: Food Packaging Film, Stationery Film, Twist Wrap Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 22.0 MPa3190 psiASTM D 882
Film Elongation at Break, MD 860 %860 %ASTM D 882
Elongation at Yield 7.0 %
@Thickness 0.0500 mm
7.0 %
@Thickness 0.00197 in
500 mm/min; ASTM D 882
Modulus of Elasticity 0.900 GPa
@Thickness 0.0500 mm
131 ksi
@Thickness 0.00197 in
25mm/min; ASTM D 882
Film Tensile Strength at Break, MD 37.0 MPa5370 psiASTM D 882
1% Secant Modulus, MD 900 MPa131000 psiASTM D 882
 
Optical PropertiesMetricEnglishComments
Haze 5.0 %
@Thickness 0.0500 mm
5.0 %
@Thickness 0.00197 in
ASTM D 1003
Gloss  45 %
@Thickness 0.0500 mm
45 %
@Thickness 0.00197 in
69 units; ASTM D 2457
 69 %
@Thickness 0.0500 mm
69 %
@Thickness 0.00197 in
45°; ASTM D 2457
 
Descriptive Properties
Processing MethodCast Film, Double Bubble

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Adstif HA 3105 Polypropylene
Dow DX5E66 Polypropylene Homopolymer Resin
PolyMirae Clyrell RC5056 Injection Molding Grade Polypropylene
LyondellBasell Moplen RP310M Polypropylene Copolymer
LyondellBasell Moplen RP2795 Polypropylene Copolymer

PEQT7024 / 218663

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.