Same as Lucryl G 88, but higher resistance to stress cracking and higher processing viscosity. Used for: extruded protective layer on PVC, ABS and PC for outdoor applications, as well as bath tubs and shower trays. Data was collected by ISO methods. Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013. |