MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV 4755B42 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 4700 Series are very high flow injection molding engineering grades with excellent UV resistance, elasticity, and surface aesthetics designed for demanding automotive applications including window encapsulation and exterior parts. This product is a black, medium hardness, low density thermoplastic vulcanizate suited for injection molding application that require superior flow properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Processability; High Flow; Low Compression Set; Low Density; Low Specific Gravity; Medium Hardness; Resilient

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Rubber Replacement

Agency Ratings: UL 94

RoHS Compliance: RoHS Compliant

Automotive Specifications: DAIMLER DBL 5422 Color: Black DAIMLER DBL 5562.30 Color: Black; FORD WSD-M2D378-A1 Color: Black; FORD WSD-M2D378-A1 Color: Natural; GM QK 003513 Color: Black; VAG VW501 23 Color: Black; VOLKSWAGEN VW 50180 Color: Black

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  54
@Time 5.00 sec
54
@Time 0.00139 hour
Extruded; ASTM D2240
 56
@Time 5.00 sec
56
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 4.30 MPa624 psiFlow; ASTM D412
 5.00 MPa725 psiAcross Flow; ASTM D412
 4.70 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
682 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 4.90 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
711 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  1.80 MPa
@Strain 100 %
261 psi
@Strain 100 %
Across Flow; ISO 37
 2.70 MPa
@Strain 100 %
392 psi
@Strain 100 %
Flow; ISO 37
 1.78 MPa
@Strain 100 %,
Treatment Temp. 150 °C
258 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
 1.93 MPa
@Strain 100 %,
Treatment Temp. 135 °C
279 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
Elongation at Break 390 %390 %Flow; ASTM D412
 500 %500 %Across Flow; ASTM D412
 480 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
480 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
 490 %
@Treatment Temp. 150 °C,
Time 605000 sec
490 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tear Strength 19.3 kN/m110 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  19 %
@Temperature 22.8 °C,
Time 79200 sec
19 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 28 %
@Temperature 70.0 °C,
Time 79200 sec
28 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 43 %
@Temperature 125 °C,
Time 252000 sec
43 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 232 °C360 - 450 °FInjection
Rear Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Middle Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Front Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Nozzle Temperature 188 - 221 °C370 - 430 °FInjection
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1162 / 237653

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.