MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Permabond A130 Anaerobic Threadlocker
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Designed for the locking and sealing of metal parts, Permabond® A130 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used to replace a wide range of mechanical locking devices. Its excellent chemical resistance makes it suitable for sealing small hydraulic and pneumatic fittings and can reduce the effects of corrosion.

Features & Benefits:

  • Excellent chemical resistance
  • Vibration resistant
  • Lubricates threads for easier assembly
  • Provides corrosion protection
  • WRAS listed for contact with wholesome (potable) water

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccUncured
Viscosity  1800 cP
@Temperature 25.0 °C
1800 cP
@Temperature 77.0 °F
at 20 rpm vibration
 8000 cP
@Temperature 25.0 °C
8000 cP
@Temperature 77.0 °F
at 2 rpm vibration
Storage Temperature 5.00 - 25.0 °C41.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 12.0 MPa1740 psisteel collar and pin shear; ISO 10123
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 11.0 kV/mm279 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°F
 
Processing PropertiesMetricEnglishComments
Cure Time  4.98 min
@Temperature 23.0 °C
0.0830 hour
@Temperature 73.4 °F
Brass, handling strength
 15.0 min
@Temperature 23.0 °C
0.250 hour
@Temperature 73.4 °F
M10 steel, handling strength
 30.0 min
@Temperature 23.0 °C
0.500 hour
@Temperature 73.4 °F
Brass, working strength
 60.0 min
@Temperature 23.0 °C
1.00 hour
@Temperature 73.4 °F
Zinc, handling strength
 60.0 min
@Temperature 23.0 °C
1.00 hour
@Temperature 73.4 °F
M10 steel, working strength
 360 min
@Temperature 23.0 °C
6.00 hour
@Temperature 73.4 °F
Stainless steel, handling strength
 360 - 1440 min
@Temperature 23.0 °C
6.00 - 24.0 hour
@Temperature 73.4 °F
Zinc, working strength
 1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
M10 steel, full strength
 
Descriptive Properties
AppearanceBlueUncured
Maximum Gap Fill (mm)0.12
Maximum Thread SizeM20
Strength Retention20% at 150°CRelative to 0°C
 70% at 100°CRelative to 0°C
 90% at 50°CRelative to 0°C
Torque Strength (N m)12M10 steel, break
 7M10 steel, prevail
UV FluorescenceYesUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERMA806 / 162731

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.