MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® F-502 Phenolic Prepreg, 3K 8HS PAN Reinforced
Categories: Polymer; Thermoset; Phenolic

Material Notes: Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rocket nozzles, as well as ducting and secondary structures. GMS4001 qualified specifications.

Key Features and Benefits:

  • Provides a combination of high-strength and ablative properties for demanding applications
  • Low thermal expansion
  • Good Tack and Drape properties
  • Conforms to MIL-R-9299 Type B

Applications/Qualifications:

  • Rocket Nozzles
  • Ducting
  • Secondary Structures

Information provided by Park Electrochemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Volatiles 2.0 - 8.0 %
@Temperature 135 °C
8 min
Thickness 16.0 milcured laminate, per ply
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 75ASTM D2583
Tensile Strength, Yield 89000 psi
@Temperature 23.9 °C
0° Direction, Dry; 325°F Autoclave Cured; ASTM D638
Tensile Modulus 8600 ksi
@Temperature 23.9 °C
0° Direction, Dry; 325°F Autoclave Cured; ASTM D638
Flexural Strength 122 ksi
@Temperature 23.9 °C
Dry; 325°F Autoclave Cured; ASTM D790
Flexural Modulus 8100 ksi
@Temperature 23.9 °C
Dry; 325°F Autoclave Cured; ASTM D790
Compressive Strength 77.0 ksi
@Temperature 23.9 °C
Dry; 325°F Autoclave Cured; ASTM D695
Compressive Modulus 9400 ksi
@Temperature 23.9 °C
Dry; 325°F Autoclave Cured; ASTM D695
Shear Strength 4.80 ksi
@Temperature 23.9 °C
Short-Beam, Dry; 325°F Autoclave Cured; ASTM D5379
 
Processing PropertiesOriginal ValueComments
Gel Time 0.800 - 3.30 min
Shelf Life 3.00 Month
@Temperature 4.44 °C
 6.00 Month
@Temperature -17.8 °C
 
Descriptive Properties
Fabric Area Weight (g/m²)617
Prepreg Resin Content (%)32-38
Resin Flow (%)10-25325°F, 15psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 1050-H14
Nanocyl PLASTICYL™ PP2001 Polypropylene with 3.2 wt% Multi-Wall Carbon Nanotubes
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/40%/193P/CHS-3K

PPARK043 / 89315

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.