MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chosun Refractories GUN-135L Light-Weight Gunning Castable
Categories: Ceramic

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  3.37e-7 - 0.00196 GPa
@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.285 ksi
@Temperature 230 °F,
Time 24.0 hour
 0.000981 - 0.001962 GPa
@Temperature 1000 °C,
Time 10800 sec
0.142 - 0.2846 ksi
@Temperature 1830 °F,
Time 3.00 hour
Compressive Strength  2.45 - 4.41 MPa
@Treatment Temp. 1000 °C,
Time 10800 sec
356 - 640 psi
@Treatment Temp. 1830 °F,
Time 3.00 hour
Cold Crushing Strength
 5.69 - 5.88 MPa
@Treatment Temp. 110 °C,
Time 86400 sec
825 - 853 psi
@Treatment Temp. 230 °F,
Time 24.0 hour
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.4653 W/m-K
@Temperature 260 °C
3.224 BTU-in/hr-ft²-°F
@Temperature 500 °F
 0.48852 W/m-K
@Temperature 540 °C
3.3849 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.55831 W/m-K
@Temperature 800 °C
3.8684 BTU-in/hr-ft²-°F
@Temperature 1470 °F
Maximum Service Temperature, Air 1350 °C2460 °Flimited
Shrinkage  -0.400 %
@Temperature 1000 °C,
Time 10800 sec
-0.400 %
@Temperature 1830 °F,
Time 3.00 hour
 -0.100 %
@Temperature 110 °C,
Time 86400 sec
-0.100 %
@Temperature 230 °F,
Time 24.0 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 37 %37 %
SiO2 41 %41 %
 
Descriptive Properties
Installation MethodGunning
Main ApplicationsFireproof insulating Part
Material Required for Estimating (kg/m3)1,450
Water Required for Casting(%)Nozzle Mixing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCHOS242 / 124186

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.