MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

MetalTek MTEK 35-15 Cast UNS N08605 Heat Resistant Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; Cast Stainless Steel; T 300 Series Stainless Steel

Material Notes: Good strength at heat treating temperatures. Resists thermal shock of repeated heating and cooling.

Applications: Dampers, pots, blades, rolls, door frames, retorts, rolling mill guides.

Information provided by MetalTek

Cast UNS N08605; Cast Grade HT; Cast ASTM A297, A351, A608; Wrought UNS N83300; Wrought Grade 330

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 179179
Tensile Strength, Ultimate >= 450 MPa>= 65300 psi
Tensile Strength, Yield >= 235 MPa>= 34100 psi
Elongation at Break >= 4.0 %>= 4.0 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 980 °C1800 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.35 - 0.75 %0.35 - 0.75 %
Chromium, Cr 15 - 19 %15 - 19 %
Iron, Fe 38.75 - 51.65 %38.75 - 51.65 %As Balance
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 33 - 37 %33 - 37 %
Silicon, Si <= 2.5 %<= 2.5 %
 
Descriptive Properties
Heat TreatmentNot Heat Treated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
330 Stainless Steel
Cast Stainless Steel HT30, UNS N08030
Cast Stainless Steel HT30, ASTM A351
Cast Stainless Steel HT30, ACI
Cast Stainless Steel HT, UNS N08002

NMETEK097 / 18347

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.