MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Latex LXC 771NA Carboxylated Styrene-Butadiene Latex  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: Applications: Dow Latex LXC 771NA is a high solids, high performance latex that offers many benefits over standard styrene-butadiene latexes in carpet applications. Dow Latex LXC 771NA is a unique product that can be used in either residential or commercial applications. The firm hand paired with high strength make it an ideal candidate in applications in which overall performance is a top priority. The firm hand characteristics produce excellent results in finishing where carpet wrinkling during production is a problem. Dow Latex LXC 771NA provides high strength and is a great choice for applications that need the highest possible tensile strength. The high solids content along with excellent dry and wet strength allow maximum formulation flexibility in both residential and commercial formulations. Although primarily used in unitary and high performance commercial backing applications, Dow Latex LXC 771NA can be used in the precoat compound for both commercial and residential carpet backing applications,

Benefits:

  • High Solids: faster drying for faster line speeds
  • Minimizes carpet wrinkling
  • Firm Hand
  • Very good wet strength
  • Blister Resistant

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/cc
Solids Content 56.5 %
Particle Size 1.53 µm
pH 7.5
Brookfield Viscosity <= 800 cP#2 @ 50 rpm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 10.0 °C
 
Descriptive Properties
Minimum film formation temperature12°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Latex LXC 8476NA Carboxylated Styrene-Butadiene Latex
KKPC KOSYN KSL 101 Styrene-Butadiene Latex
Mallard Creek Polymers Tylac® 4190 SBR Emulsion
Mallard Creek Polymers Rovene® 9410 Carboxylated Styrene-Butadiene Emulsion
Versalis Europrene Latice® B 010 Styrene - Butadiene Copolymer

PDWST096 / 142305

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.