MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Von Roll Durapol® M600 SMC Polyester - Glass Laminate
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer, Glass Filled

Material Notes: Highlights: Dimensional stability, halogen-free 94V-0.

Glass mat laminates are manufactured using low-pressure techniques and are characterized using mainly glass mat or chopped glass as a reinforcement material. Delmat® and Durapol® laminates are widely used in the electro-mechanical industries. Von Roll has also developed special qualities for the electronics industry and for thermal protection applications. The products are attractive both for their good mechanical and electrical properties, and their resistance against corrosion at high-temperature levels.

Information provided by Von Roll.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 - 2.00 g/ccISO 1183
Water Absorption 0.10 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 150 MPaISO 527
Flexural Strength 120 MPa
@Temperature 155 °C
flatwise; ISO 178
 250 MPa
@Temperature 23.0 °C
flatwise; ISO 178
Compressive Strength 400 MPaflatwise; ISO 604
Charpy Impact, Notched 120 kJ/m²Edgewise; IEC 60893-2
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 1.00e+11 ohmafter immersion in water; IEC 60167
Dielectric Strength 12.0 kV/mmflatwise; IEC 60243-1
Dielectric Breakdown 60000 VTaper pin electrodes, edgewise; IEC 60243-1
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°C
Maximum Service Temperature, Air 155 °CTemperature Index; IEC 60216
Flammability, UL94 V-0
 
Descriptive Properties
ColorSimilar to Green RAL 6019
ReinforcementChopped glass fibers + roving.
Sheet Size (mm)2000 x 1250

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVONR9930 / 249220

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.