Bapolene 1057EC is a low density polyethylene for high speed extrusion coating applications that require superior adhesion and neck-in. This product meets US FDA 21 CFR 177.1520. Applications: Packaging; Paper Coatings; Pouches - Flexible Packaging. Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers |
Food Contact Acceptable; Good Adhesion; Low Neck-In. |