MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Marco Polo MARPOL EVA 28800 EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: MARPOL ® EVA 28800 is low viscosity Vinyl Acetate copolymer designed for enhanced tensile performance. This resin has good compatibility with hydrocarbons, most waxes, and natural tackifiers for making hot melt adhesives, sealants and wax blends.

Recommended Applications: Adhesives, sealants, hot melt adhesives, industrial sealants, glue sticks, low viscosity adhesives.

Additives: Antiblock – no, Slip – no, Thermal Stabilizer.

Form(s): Pellets.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.953 g/cc0.0344 lb/in³ASTM D1505
Viscosity 9300 cP
@Temperature 190 °C
9300 cP
@Temperature 374 °F
ASTM D3236
Vinyl Acetate Content 27.6 %27.6 %
Melt Flow 800 g/10 min
@Load 2.16 kg,
Temperature 190 °C
800 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6969ASTM D2240
Hardness, Shore D 1818ASTM D2240
Tensile Strength at Break 2.07 MPa300 psiASTM D638
Elongation at Break 360 %360 %ASTM D638
Flexural Modulus, 1% Secant 20.0 MPa2900 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 68.0 °C154 °FPeak; ASTM D3418
Vicat Softening Point 50.0 °C122 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO222 / 283819

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.