TE Series highly transparent ABS resins have excellent color attributes and tensile strength. TE is superior to polycarbonates in terms of moldability and flexibility, and besides are characterized by low density. Used for electronic equipment and components, information equipment components, AV equipment, etc.Information provided by Denka Company Limited. |