High viscosity (200 RV), extrusion grade nylon 6/6 recommended for practically all types of extrusion including profile, film and extrusion coating. Has good melt flow and melt strength properties. Optimum processing conditions should permit for a melt temperature of 550°F -575°F at the die. Testing conducted on dry as molded specimen at 73°F Information provided by Nylene® Global Polymer Solutions. |