Data provided by the manufacturer, Exxon Chemical. A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 363C32 resin have outstanding tensile properties and impact and puncture toughness. Applications: Cast stretch film. Data for film properties below based on 0.8 mil film. |
Low Density Polyethylene; Exxon Chemical Company |