MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ChenGuang 941 Silicone Resin
Categories: Polymer; Thermoset; Silicone

Material Notes: Properties:
  • Silicone resin are mixtures of solvent (toluene or xylene) with combined hydrolyzates of methyl chlorosilanes and phenyl chlorosilanes contain some amount of hydroxyl groups. The hydroxyl can further condensed into a hard film under heating. Solid content is 50~70% on sale.
  • Outstanding insulation property, high-and-low-temperature resistance, corona and electric arc
  • resistance, water-proof. Outstanding resistance to weather-aging, ozone and chemicals.
  • With silicone resin, the H-grade motor, other electric appliances would be size-small, weight-light, last-long and could be used under harsh environment.
  • When over loaded, the motor or other electric appliance would not go out of order and would not burn heavily. The gasses giving off are not poisonous. The remains after burning is silicon dioxide.
Main Applications: Painted glass fabric lamination, etc

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content >= 56 %
@Temperature 180 °C,
Time 86400 sec
 
Processing PropertiesOriginal ValueComments
Dry Time >= 0.4167 hour
@Temperature 110 °C
no copper
Shelf Life >= 3.00 Month
 
Descriptive Properties
AppearanceLight-yellow to brown solution
Heat Resistance<7hrPainting solidification time, 200°C on copper sheet
Weight Loss<5%at 250°C, 3hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHENGU069 / 255668

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.