MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elmet Technologies UX 5 Pure Tungsten Powder
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy; Pure Element

Material Notes: Elmet Technologies manufactures high quality tungsten metal powders for use in mill products, tungsten heavy alloys, electrical contacts, electrodes, transducers, sputtering targets, tungsten-polymer compounds, and metal injection molded products.

Information provided by Elmet Technologies.

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density >= 4.27 g/cc>= 0.154 lb/in³Scott
 >= 7.50 g/cc>= 0.271 lb/in³Tap
Particle Size 4.5 - 5.5 µm4.5 - 5.5 µmFSSS particle size, as-supplied
Particle Mesh Size 150 Mesh150 Mesh
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0020 %<= 0.0020 %
Chromium, Cr <= 0.0020 %<= 0.0020 %
Copper, Cu <= 0.0010 %<= 0.0010 %
Iron, Fe <= 0.0050 %<= 0.0050 %
Molybdenum, Mo <= 0.0050 %<= 0.0050 %
Nickel, Ni <= 0.0040 %<= 0.0040 %
Other, each <= 0.0020 %<= 0.0020 %
Oxygen, O 0.020 %0.020 %
Potassium, K <= 0.010 %<= 0.010 %
Silicon, Si <= 0.0020 %<= 0.0020 %
Sodium, Na <= 0.0020 %<= 0.0020 %
Tungsten, W >= 99.95 %>= 99.95 %
 
Descriptive Properties
REACH ComplianceRegulation (EC) No. 1907/2006
RoHS Compliance2002/95/EC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NELMET929 / 242050

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.