MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

MOL Group TIPELIN 1100J HDPE, Injection molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Description: TIPELIN 1100J is a high density unimodal polyethylene copolymer (with propene-1 as comonomer) intended for injection molding of general purpose products. It offers good balance of properties between stiffness and processability. The grade contains antioxidant and acid scavenger.

Applications: TIPELIN 1100J is recommended for making daily necessaries, kitchen housewares, boxes, crates, trays, toys, caps, cartridges.

(1) Average mechanical property values of several measurements carried out on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). (2) Average mechanical property values of several measurements carried out on standard injection molded specimens (ISO 294-1) conditioned at room temperature (ISO 291).

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.961 g/cc0.0347 lb/in³1; ISO 1183-2
ESCR 100% Igepal® 3.0 hour3.0 hour1, CO-630; ASTM D 1693
Oxidative Induction Time (OIT) 30 min
@Temperature 200 °C
30 min
@Temperature 392 °F
EN 728
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 63632; ISO 868
Tensile Strength at Break 10.0 MPa1450 psi2; ISO 527-1,2
Tensile Strength, Yield 28.0 MPa4060 psi2; ISO 527-1,2
Elongation at Break 750 %750 %2; ISO 527-1,2
Elongation at Yield 11 %11 %2; ISO 527-1,2
Flexural Modulus 1.40 GPa203 ksi1; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²1; ISO 180/A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 128 °C262 °F1; ISO 306/A 120
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 - 250 °C410 - 482 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG067 / 297233

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.