MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ LUBRICOMP™ Compound KP004XXP Acetal (POM) Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: LNP LUBRICOMP KP004XXP compound is based on Acetal (POM) Copolymer resin containing 20% PTFE/silicone. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ASTM D792
 1.48 g/cc0.0535 lb/in³ISO 1183
Moisture Absorption 0.180 %0.180 %23°C/50% RH/24 hrs; ASTM D570
 0.430 %0.430 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.021 - 0.029 cm/cm0.021 - 0.029 in/in24hrs; ASTM D955
 0.0209 - 0.0292 cm/cm0.0209 - 0.0292 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.021 - 0.029 cm/cm0.021 - 0.029 in/in24hrs; ASTM D955
 0.0209 - 0.0292 cm/cm0.0209 - 0.0292 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 39.0 MPa5660 psiISO 527
 43.0 MPa6240 psiASTM D638
Tensile Strength, Yield 39.0 MPa5660 psiISO 527
 43.0 MPa6240 psiASTM D638
Elongation at Break 30.3 %30.3 %ASTM D638
 42.8 %42.8 %ISO 527
Elongation at Yield 13.7 %13.7 %ASTM D638
 21.5 %21.5 %ISO 527
Tensile Modulus 1.83 GPa265 ksi50 mm/min; ASTM D638
 2.02 GPa293 ksi1 mm/min; ISO 527
Flexural Strength 60.0 MPa8700 psiISO 178
 63.0 MPa9140 psiASTM D790
Flexural Modulus 2.02 GPa293 ksiASTM D790
 2.08 GPa302 ksiISO 178
Izod Impact Notched 53.0 J39.1 ft-lbASTM D256
Izod Impact, Unnotched 6.19 J/cm11.6 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 42.0 kJ/m²20.0 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 J2.21 ft-lbpeak; ASTM D3763
Impact Test 1.00 J0.738 ft-lbMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.250.25ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.140.14ASTM D3702 Modified: Manual
K (wear) Factor 18.1 x 10-8 mm³/N-M9.00 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  111 µm/m-°C
@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 111 µm/m-°C
@Temperature -40.0 - 40.0 °C
61.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  114 µm/m-°C
@Temperature -40.0 - 40.0 °C
63.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 114 µm/m-°C
@Temperature -40.0 - 40.0 °C
63.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C174 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 87.0 °C
@Thickness 3.20 mm
189 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 195 - 205 °C383 - 401 °F
Zone 3 210 - 220 °C410 - 428 °F
Melt Temperature 200 - 215 °C392 - 419 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80867 / 288814

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.