MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Shandong Dongyue Shenzhou New Material Co CHF115 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Conformable with: Q/DYS 001-2007

Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton exchange membrane fuel cells, lithium-ion rechargeable batteries, other fields such as electrolysis devices, sewage disposal, chemical catalysis, photocatalysis, gas separation, functional composite materials, particular electrical active polymers used for robot.

Main Applications:

The resin can be used to produce ion exchange conductive membrane, fuel cell proton ion membrane, super acid catalyst, super stable ion-exchange agent, etc.

Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.93 - 2.03 g/ccResin
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature >= 350 °C
 
Descriptive Properties
AppearanceTranslucent granular
Exchange Capacity (IEC) (mmol/g)1.13-1.17
Group FormulaRf-SO2F, RF-SO3Na, Rf-SO3H

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSHEN036 / 104091

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.