MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bamberger Polymers Bapolene® 3042 BLK Polyethylene, Rotational Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Bapolene LL3042 BLK is a black LLDPE resin specifically designed for rotational molding applications. It offers excellent environmental stress cracking resistance, warp resistance, and impact strength. It is available in pellet or powder form. UV stabilized. This product meets FDA standards for food contact applications.

Applications: Large rotational molded parts such as industrial and agricultural outdoor storage tanks, drums, and trash cans.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Excellent environmental stress cracking resistance, warp resistance, and impact strength
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.936 g/cc0.0338 lb/in³ASTM D1505
Environmental Stress Crack Resistance >= 450 hour>= 450 hourASTM D-1693; at 10% Igepal
 >= 1000 hour>= 1000 hourCondition B, F50, 100% Igepal; ASTM D-1693
Melt Flow 5.5 g/10 min5.5 g/10 min190°C/2160g; ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 15.2 MPa2200 psi2 in/min (50 mm/min); ASTM D638
Elongation at Break 450 %450 %2 in/min (50 mm/min); ASTM D638
Flexural Modulus 0.610 GPa88.5 ksi2% Secant; ASTM D-790
Impact Test 67.8 J50.0 ft-lbARM Impact; 1/8" specimen, 176 ft-lbs. at 1/4" specimen; -40°C
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 51.0 °C124 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 37.0 °C98.6 °FASTM D-648
Vicat Softening Point 110 °C230 °FASTM D1525
 
Descriptive Properties
processRotational Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBP3B150 / 20807

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.